I think it’s either US or German built, no idea though.
Yeah, I’ll owe about 5k fed tax and my W4 is set up so I usually pay/owe nothing come tax time… so I’d currently get about a 5k refund. I’m looking at ways to increase my federal taxes before EOY to squeeze more out of it.
Dang, I need to try that. Good idea.
It might just be the specific spool/brand of PETG you used. Try buying some from a major well-known manufacturer, like Overture, Polymaker, etc. I’ve had cheaper brands shrink, warp, have adhesion issues, and all sorts of other quirks.
Make sure it’s from one of Sunlu’s official stores… aliexpressis pretty shady lol.
Nope, this is the same size as the stock Prusa sheets. The sheets are all a little bigger than the actual build area.
This is just a regular-sized Prusa MK4, 250 x 210mm xy build area. I made this custom magnetic G10 sheet for printing PETG, it’s 253.8 x 241mm.
You could also mess with your retraction settings to try and reduce stringing.
I had one weird roll of PETG that could only be printed at lower temperatures, so it’s possible. Still looks like the filament is wet to me… I recommend picking up a Sunlu S1 Plus when it drops under $40, I like being able to both dry the spool and print straight from the dryer (only takes a couple hours to re-absorb moisture).
Ended up moving the little 500VA UPS from my computer to the 3D printer. Hopefully it’ll help for brief blips.
This model was set up for it already in the .3mf file. It stops, moves the toolhead over, automatically unloads the filament, and waits for me to yank it the rest of the way out then stick in another color. It then purges the nozzle a bit to get the main color fully flowing and asks you if it’s correct before proceeding. I did this like 7 times for this stupid half-failed box lol.
Edit: Also, you can left-click the plus sign on the layer slider at any height you want after slicing in PrusaSlicer to add manual color changes in.
This could be it, OP should check what the actual temperature says on the screen during printing.
Aside from drying, here are some thoughts:
Double-check the print temperature, PETG should be about 240-ish. Also the spiral vase mode may be the issue if your model isn’t designed for it. Also check your z offset, the first layer should be almost a flawless sheet… if not, stop the print and try again while live adjusting the z until it’s correct. Typically PETG doesn’t like to be squished down as much as PLA.
I printed the panels using the full width of my large 300x300mm print bed. I have three of them mounted to the wall. There are several sizes available though, you can always merge more smaller ones.
It’s actually just a shorter version of the tall basket model that was available. I originally meant for it to hold my alcohol bottle, but it was too small… then I discovered it fits the canned air perfectly.
It’s a good system. There are an insane number of tool holders already available for download, and it’s pretty easy to design your own by sticking the existing male hexagon part onto a model in fusion 360. Note the direction of the hexagons when mounting the panels… I had these rotated 90 degrees at first without realizing, which means all of my tool holders would have been at the wrong angle lol. Had to patch some holes and remount the panels, ugh.
Don’t question my methods lol
The hexagon panels have a larger recess in the back, so parts snap in securely.
Neat, good job. You might want to include what screw size it fits, and the word “anchor” somewhere in the description/title for searching (these are typically called drywall anchors in the US).
Enclosure is mostly to keep cat hair off my printer (my cat sheds like crazy) and to filter some of the microplastic dust and fumes. It does reduce warping by keeping the volume warmer than room temperature, I print a lot of PETG so this helps.